Product Detail
Alnico magnets, composed of primarily aluminum, nickel, and cobalt, were developed in the 1940's. This class of magnet remains a preferred material because of it's excellent temperature stability, high magnetic flux density, and resistance to corrosion. Alnico magnets are manufactured through a casting or sintering process. The casting process allows for the magnet to be manufactured into intricate and complex shapes, which are not possible with other magnetic materials.
Alnico Magnets Overview
Alnico magnetic material is an alloy of aluminum-nickel-cobalt which possesses an excellent temperature stability and high residual induction. However, its low coercive force limits its applications in many cases. Casting and sintering are two major processes used to manufacture the Alnico magnets.
Performance of Cast Alnico Magnets
CharacterIstics Model | Max. Energy Product | Br (Residual induction) | Hcb (Coercive Force) | Hcj (Intrinsic coercive Force) | Density | Temp.Coeffienct of Br. | Curie point | Remark |
| (MGOe) | (KGs) | (KOe) | (KOe) | g/cm3 | %/K | °C | Isotropic |
SAlNiCo4/1 | 0.40-0.60 | 8.7-8.9 | 0.11-0.14 | 0.13-0.15 | 6.8 | -0.02 | 750 |
SAlNiCo8/5 | 1.07-1.19 | 5.3-6.2 | 0.57-0.63 | 0.59-0.65 | 6.8 | -0.02 | 750 |
SAlNiCo10/5 | 1.19-1.38 | 6.3-7.0 | 0.63-0.73 | 0.63-0.73 | 6.8 | -0.02 | 780 |
SAlNiCo12/5 | 1.38-1.63 | 7.0-7.5 | 0.62-0.70 | 0.66-0.73) | 7.0 | -0.02 | 800 |
SAlNiCo14/5 | 1.63-1.88 | 7.3-8.0 | 0.59-0.63 | 0.63-0.67 | 7.1 | -0.02 | 790 |
SAlNiCo14/6 | 1.76-2.00 | 6.2-8.1 | 0.70-0.81 | 0.73-0.83 | 7.1 | -0.02 | 790 |
SAlNiCo14/8 | 1.76-2.00 | 5.5-6.1 | 0.94-1.11 | 1.00-1.16 | 7.1 | -0.01 | 850 |
SAlNiCo18/10 | 2.00-2.39 | 5.7-6.2 | 1.16-1.26 | 1.24-1.34 | 7.2 | -0.01 | 860 |
SAlNiCo29/6 | 3.64-4.15 | 9.7-12 | 0.73-0.80 | 0.75-0.83 | 7.2 | -0.02 | 860 | Anisotropic |
SAlNiCo30/6 | 3.77-4.27 | 10-11 | 0.73-0.80 | 0.75-0.83 | 7.2 | -0.02 | 860 |
SAlNiCo42/10 | 5.27-5.77 | 9.5-11 | 1.26-1.38 | 1.30-1.43 | 7.2 | -0.01 | 860 |
SAlNiCo33/11 | 4.14-4.77 | 7-8 | 1.34-1.45 | 1.39-1.50 | 7.2 | -0.01 | 860 |
SANiCo35/5 | 4.40-4.90 | 11-12 | 0.60-0.65 | 0.63-0.68 | 7.2 | -0.02 | 850 |
SAlNiCo37/15 | 4.65-5.15 | 7.0-8.0 | 1.76-1.85 | 1.88-1.98 | 7.2 | -0.01 | 870 |
SAlNiCo39/12 | 4.90-5.40 | 8.3-9.0 | 1.45-1.54 | 1.50-1.60 | 7.25 | -0.01 | 860 |
SAlNiCo44/12 | 5.53-6.03 | 9-9.5 | 1.50-1.60 | 1.56-1.66 | 7.25 | -0.01 | 860 |
SAlNiCo40/15 | 5.02-6.03 | 7.5-8.5 | 1.80-1.90 | 1.95-2.05 | 7.2 | -0.01 | 870 |
SAlNiCo44/15 | 5.53-6.03 | 8.0-8.8 | 1.86-2.00 | 1.95-2.05 | 7.2 | -0.01 | 870 |
Performance of Cast Alnico Magnets
Characteristics Model | Max. Energy Product | Br (Residual induction) | Hcb (Coercive Force) | Hcj (Intrinsic coercive Force) | Density | Temp.Coeffienct of Br. | Curie point | Remarks |
| (MGOe) | (KGs) | (KOe) | (KOe) | g/cm3 | %/K | °c | Isotropic |
AlNiCo12/6 | 1.50 | 6.4 | 0.65 | 0.70 | 7.0 | -0.03 | 810 |
AlNiCo13/6 | 1.63 | 7.5 | 0.65 | 0.70 | 7.0 | -0.03 | 810 |
AlNiCo18/10 | 2.26 | 5.3 | 1.13 | 1.22 | 7.1 | -0.01 | 860 |
AlNiCo20/11 | 2.51 | 6.0 | 1.26 | 1.36 | 7.3 | -0.01 | 860 |
AlNiCo36/6 | 4.52 | 11.5 | 0.75 | 0.78 | 7.3 | -0.02 | 850 | Anisotropic |
AlNiCo38/5 | 4.77 | 12.0 | 0.63 | 0.65 | 7.3 | -0.02 | 850 |
AlNiCo40/5 | 5.03 | 12.5 | 0.62 | 0.63 | 7.3 | -0.02 | 850 |
AlNiCo44/5 | 5.53 | 12.7 | 0.65 | 0.67 | 7.3 | -0.02 | 850 |
AlNiCo52/6 | 6.53 | 13.0 | 0.71 | 0.72 | 7.3 | -0.02 | 850 |
AlNiCo60/6 | 7.54 | 13.5 | 0.74 | 0.75 | 7.3 | -0.02 | 860 |
AlNiCo38/11 | 4.77 | 8.5 | 1.38 | 1.41 | 7.3 | -0.01 | 860 |
AlNiCo40/17 | 5.02 | 7.5 | 1.96 | 2.11 | 7.3 | -0.01 | 870 |
AlNiCo46/12 | 5.78 | 9.3 | 1.51 | 1.56 | 7.3 | -0.015 | 860 |
AlNiCo48/16 | 6.03 | 8.2 | 1.81 | 1.98 | 7.3 | -0.01 | 870 |
AlNiCo72/12 | 9.04 | 10.5 | 1.43 | 1.46 | 7.3 | -0.015 | 850 |
AlNiCo80/12 | 10.04 | 10.8 | 1.51 | 1.53 | 7.3 | -0.015 | 850 |
Key Advantages
Excellent temperature stability
Strong corrosion resistance
The maximum working temperature is up to 500°c
Excellent capacity
High density and magnetic properties
Shorter production lead time
Temperature factor of Br is the smallest among all the permanent magnets
Cast Alnico magnets can be produced in relatively complex shapes
Tooling for cast Alnico magnets is relatively low, since sand molds are generally used for the casting process.
Common Applications
Holding magnets Separators Sensors Security systems MRI Relays Magnetos
Address:
Zhong Nan Gao Ke 18 Building, Dongligu, Tianyuan, Zhuzhou, Hunan, China
Business Type:
Manufacturer/Factory, Trading Company
Business Range:
Auto, Motorcycle Parts & Accessories, Electrical & Electronics, Instruments & Meters, Manufacturing & Processing Machinery, Metallurgy, Mineral & Energy, Sporting Goods & Recreation, Tools & Hardware, Transportation
Company Introduction:
Zhu Zhou Summit New MAterials Co. Ltd was founded in 2009, as a professional manufacturer and exporter, We are specialized in producing of rare earth magnet with the capacity of 1000 ton/year, including the grade of sintetred NdFeB magnet such as N52 N50M N48H N45SH N40UH N38EH N33AH. Great block magnets of N45H (6"X4"X2") for magnetic suspension, Big ring magnets N42M (OD100 OD120 OD150 OD160 OD200) for magnetic separator, All kinds of complicated shape of arc magnets for automotive motor and wind power generator are competitive.
In 2023, Summit build up new workshop to produce permanent magnet motor ( BLDC motor and PMSM motor ), it can produce SL 9050 IPM motor, SL 120-30/35/40/50/60/80 SL 140 IPM, SL 180 IPM PMSM motor and BLDC motor for electric motorcycle, Ebike, E go kart, E skate board And Summit Co, provide Fardrive controller, Sabvoton, Kelly Controller to run PMSM motor
Our purpose " Honesty, Professional, Mutual Benefit